Experiment de măcinare cu oxid de siliciu (SiO2).
fundaluri: Ground by Tencan planetary ball mill matched with agate jars and agate balls. After 2 hours of grinding, granularity of output powder meets customer’s request.
Masina aplicata: Moara planetara verticala cu bile Tencan Model Nr.XQM-0.4
1. descriere
1) Applied Field: Silicon Material.
2) Materials: Silicon Oxide.
3) Feed Size: 1-5mm
4) Cantitatea de furaj: 100g
5) Property of Material: Hard and Crispy
6) Solicitarea clientului: Sub 50μm.
7) Analiză ulterioară: Testul mărimii particulelor ⇒
Before Grinding After Grinding
2. Soluții
1) Selecția echipamentului: Moara cu bile planetară verticală Model XQM-0.4
2) Accessories: 50ml Agate Jars and 5-10mm Agate Balls.
3) Setarea parametrilor de rulare: Viteza de rotație: 560 rpm, funcționare reciprocă pozitivă și negativă la fiecare 30 de minute de funcționare.
4) Timp de măcinare: 2 ore
5) Rezultat măcinare: 100% <50μm
6) Conclusion: Planetary Ball Mill Model XQM-1 can be used to grind silicon oxide.
3. Câmpuri de aplicare: Silicon material of solar cell industry.